Glass paste for automobiles
Pick up:
Dipping test into sulfuric acid solution : Pass for 4 hours Firing temperature: 570 to 640 deg C
Excellent antistick Firing temperature: 600 to 660 deg C
Dipping test into sulfuric acid solution : Pass for 4 hours Firing temperature: 610 to 640 deg C Excellent antistick
Dipping test into sulfuric acid solution : Pass for 4 hours Firing temperature: 580 to 620 deg C Excellent antistick
Dipping test into sulfuric acid solution : Pass for 4 hours Firing temperature: 640 to 660 deg C For shallow bending
Dipping test into sulfuric acid solution : Pass for 4 hours Firing temperature: 660 to 700 deg C For deep bending Excellent antistick
Dipping test into sulfuric acid solution : Pass for 140 hours (High acid resistance) Firing temperature: 620 to 660 deg C For shallow bending
Dipping test into sulfuric acid solution : Pass for 140 hours (High acid resistance) Firing temperature: 640 to 680 deg C For deep bending Excellent antistick
Dipping test into sulfuric acid solution : Pass for 4 hours Firing temperature: 620 to 660 deg C For shallow bending
GLASS COLOR, dipping test into sulfuric acid solution: Pass for 72 hours Firing temperature: 640 to 680 deg C For deep bending