Glass paste for automobiles
PFBW-2397KZC
PFBW-2397KZC
Dipping test into sulfuric acid solution
: Pass for 140 hours (High acid resistance)
Firing temperature: 640 to 680 deg C
For deep bending
Excellent antistick